Graphene dispersion sample in a lab beaker

Most graphene additive trials that fail do not fail because of the graphene. They fail because the test could not show a difference: no baseline, too many changes at once, or the wrong measurement. This guide sets out a simple, repeatable plan that works across our products, from lubricants to coatings to polymers. Product-specific details are in the individual guides linked below.

Step 1: Define the question

Write down one sentence: "We want to know whether adding graphene to [product] improves [property], measured by [test]." For example, wear scar in a four-ball test, compressive strength of cylinders, or lap-shear strength of bonded joints. If you cannot write that sentence, the trial is not ready.

Step 2: Choose a baseline

Use a product you already make, with existing data from the same test. The baseline is what makes the result meaningful. Make a fresh baseline batch alongside the treated batches rather than relying only on old data, since materials and equipment drift.

Step 3: Tell us the system

We need to match the carrier to your product. Tell us:

  • The product and its continuous phase: water, solvent, resin or oil.
  • Your mixing method and temperatures.
  • Other additives, dispersants or fillers present.
  • The property you want to improve and the test you will use.

Our guide to choosing a graphene dispersion carrier explains why this matters.

Step 4: Set the dose

Most of our additives are dosed at 1% to 7% by weight, depending on the job. Run two or three levels around the starting point we suggest, for example a low, middle and high rate. One level tells you little; several show a trend. Concrete is the exception: NanoTechCrete is dosed at 5% of cement weight, for lab samples and plant or truck loads. Reduce mix water by the same weight.

Step 5: Change one thing

Keep everything except the additive the same: raw material lots, batch size, mixing time, temperatures, cure and conditioning. If the additive brings liquid with it, adjust the formula so the solids or water content matches the baseline. Record everything.

Step 6: Mix properly

Our additives are pre-mixed, so they do not need special equipment, but they do need to be mixed until uniform. Shake or stir the container before use, add it at the point we recommend, and mix for at least as long as your usual process. Check for streaks, specks or settling.

Step 7: Measure what matters

  • Primary property: the one in your question.
  • Processing: viscosity, cure, flow or anything that affects production.
  • Side effects: properties that could get worse, such as impact strength, colour, electrical insulation or filterability.
  • Repeatability: enough specimens per batch to see whether a difference is real.

Use the same recognised test methods as your baseline data. For lubricants that often means ASTM D4172 and D2783; for concrete, ASTM C39. Our lubricant test article explains those methods.

Step 8: Read the results honestly

  1. Compare treated batches with the fresh baseline, not just with old data.
  2. Look at the spread of results, not only the average.
  3. Check whether the effect grows with dose. A trend is more convincing than one good number.
  4. Note any side effects, good or bad.
  5. Decide the next step: adjust the dose, change the carrier, scale up or stop.

Step 9: Scale up carefully

A lab result is a starting point. Before production, run a pilot batch on production equipment and repeat the key tests. Check storage stability of the finished product too.

Product guides

Documenting the trial

Good records make results useful later. For every batch, record the additive lot, dose, base material lots, mixing method and time, temperatures and test dates. Keep retained samples. If you share results with us, we can help interpret them and suggest the next step. Standard practice for interlaboratory comparisons, such as ASTM E691 on precision of test methods, is a reminder that every test has scatter; know how much yours has before you read a small difference as real.

Common reasons a trial is inconclusive

  • The additive was not mixed in fully, or settled before use.
  • The carrier did not match the product, so graphene came out of dispersion.
  • Only one specimen per batch, so normal scatter hid the effect.
  • Something else changed between baseline and treated batches.

Browse our graphene products, read the lubrication press release, or request samples for a trial.

Frequently asked questions

How much graphene additive should I use in a trial?

Most of our additives are dosed at 1% to 7% by weight, depending on the job. Run two or three levels. Concrete is dosed at 5% of cement weight, for lab samples and plant or truck loads. Reduce mix water by the same weight.

Why do I need a fresh baseline?

Materials and equipment drift. A baseline batch made alongside the treated batches is the fairest comparison.

Do I need special mixing equipment?

No. Our additives are pre-mixed. Mix until uniform with your normal equipment.

What if the trial shows no improvement?

Check dispersion, dose and carrier match first, then talk to us. Sometimes graphene is not the right tool, and we will say so.

Request a quote, samples or a spec sheet

Tell us your material, the property you want to improve, the carrier you use (water, solvent, resin or oil) and your volumes. Pricing and samples are by quote. Call 704-659-3682 or request a quote, samples or a spec sheet / SDS.

For concrete applications, explore strength-tested mixes and embodied carbon, including a conditional cement-production calculation—not a measured GI carbon saving. Explore the concrete and embodied-carbon guide.

Choose evidence for the product you are developing

Match the evidence to the application: a lubricant wear-scar result, a water-loop heat-transfer result and a concrete strength result answer different questions. Compare your own formulation at the required performance, then measure energy, material use and service needs, including additive and carrier impacts.

Lubricant test evidence · ThermaGraph / ThermaGraph-D · Concrete and embodied carbon